Exterior paint fails for one of two reasons: it was applied in the wrong conditions, or it was applied to a surface that was never going to hold it. Preparation is the unglamorous half of the job and it decides whether the coating lasts three years or twelve.
How should the wall be cleaned?
Start by removing everything loose. A stiff brush over the whole elevation dislodges flaking paint, surface dirt and cobwebs and tells you a great deal about the condition of what is underneath.
Pressure washing is effective on sound render and pebbledash, though it needs restraint. Keep the lance moving, work at a moderate pressure and hold it at an angle rather than driving water straight into the surface. Sound render tolerates this easily. Soft or already failing render will be stripped away, which is useful information but not what most people intend.
What should you do about green algae?
Washing it off does not deal with it. Algae, lichen and mould have root structures within the surface, and cleaning removes the visible growth while leaving the organism to return within months, often through the fresh paint.
Apply a proprietary fungicidal wash after cleaning, leave it for the time stated on the container, usually several hours or overnight, and rinse or brush off as instructed. North-facing walls, areas shaded by trees and anywhere near a leaking gutter will need this treatment and will need it again in future, so fixing the underlying moisture source matters as much as the chemical.
How do you tell if a surface needs stabilising?
Rub a hand firmly over the dry wall. If it comes away chalky and coloured, the existing coating has degraded to powder and new paint applied over it will bond to that loose powder rather than to the wall.
A stabilising solution is a thin, penetrating primer that soaks into the friable surface and binds it together. It is essential on chalky old masonry paint, on bare and porous render and on any surface that fails the hand test. Skipping it is the single most common reason a newly painted wall peels in sheets after one winter.
What needs repairing before you paint?
- Hairline crazing, which can usually be bridged by a textured masonry paint
- Cracks over about two millimetres, which need an exterior grade flexible filler
- Hollow-sounding render, which has lost its bond and must be cut out and replaced
- Open joints around window and door frames, which need exterior sealant rather than filler
- Defective pointing, which should be raked out and repointed before any coating goes on
Tap the render across the elevation with the handle of a screwdriver as you go. A dull, hollow note indicates the render has separated from the wall behind, and painting over it simply seals a problem that will grow.
Why does damp need fixing first?
Paint applied over a wall that is wet from an ongoing source will blister, regardless of the product. Common sources are leaking gutters and downpipes, cracked render allowing water in behind, a blocked or bridged damp proof course, and ground levels raised above the damp proof course by a patio or flowerbed.
All of these need resolving before decoration, and the wall then needs time to dry out. Freshly repointed brickwork or new render needs several weeks and sometimes months, depending on thickness and weather. Painting it early traps moisture behind the film.
What should be masked or removed?
Take down what you can rather than painting around it. House numbers, light fittings, hanging baskets, satellite brackets and alarm boxes are usually easier to remove and refit than to cut in around neatly.
Mask window frames, sills, gutters and downpipes with exterior grade tape, and protect paths, patios and planting with dust sheets rather than plastic, which becomes lethal underfoot when wet. Masonry paint on a paving slab is extremely difficult to remove once it has cured, so spending twenty minutes protecting the ground is time well spent before you open the first tin.